PETG82% confidence
Best Settings for Prusament Prusament PETG 1.75mm on Anycubic Kobra 2
Nozzle 240°C · Bed 80°C · 80 mm/s
Anycubic Kobra 2 Specs
- Max Nozzle Temp
- 260°C
- Max Bed Temp
- 90°C
- Hotend Type
- PTFE-lined
- Default Nozzle
- 0.4 mm
- Build Volume
- 220×220×250 mm
- Enclosure
- Open frame
- Release Year
- 2023
Prusament Prusament PETG 1.75mm Specs
- Material
- PETG
- Nozzle Temp Range
- 230°C – 250°C
- Bed Temp Range
- 70°C – 90°C
- Diameter
- 1.75 mm
- Spool Weight
- 1000 g
High-quality PETG with tight tolerances. Excellent layer adhesion, chemical resistance, and durability. Great for functional parts that need more strength than PLA.
Print Settings
0.4 mm nozzle· 0.2 mm layer height
82% confidenceSource: Community
Nozzle Temp
240°C
1st: 245°C
Bed Temp
80°C
1st: 80°C
Print Speed
80 mm/s
1st: 20 mm/s
Fan Speed
40%
| Parameter | Value |
|---|---|
| Nozzle Diameter | 0.4 mm |
| Layer Height | 0.2 mm |
| Nozzle Temperature | 240°C |
| Bed Temperature | 80°C |
| Print Speed | 80 mm/s |
| Retraction Distance | 5.5 mm |
| Retraction Speed | 45 mm/s |
| Fan Speed | 40% |
| Enclosure | Optional |
Notes
Kobra 2 + Prusament PETG: Bowden needs 5.5mm retraction. PTFE-lined hotend limits max temp — 240°C is fine for PETG. 40% fan.
Where to Buy Prusament Prusament PETG 1.75mm
Prusament
Prusament PETG 1.75mm
Check price on PrusaBuy on Prusa
* Affiliate links — we may earn a commission at no extra cost to you. Learn more.
Related Settings
Other filaments on the Anycubic Kobra 2
Prusament Prusament PETG 1.75mm on other printers
Frequently Asked Questions
What nozzle temperature should I use for Prusament Prusament PETG 1.75mm on the Anycubic Kobra 2?
The recommended nozzle temperature is 240°C, with a first layer temperature of 245°C. This is based on a confidence score of 82%.
What bed temperature should I use for PETG on the Anycubic Kobra 2?
Set your bed temperature to 80°C, with 80°C for the first layer.
What print speed should I use for Prusament Prusament PETG 1.75mm?
The recommended print speed is 80 mm/s, with a slower first layer speed of 20 mm/s.
Does printing PETG on the Anycubic Kobra 2 require an enclosure?
No, an enclosure is not strictly required for printing PETG on the Anycubic Kobra 2, though it can help in cold environments.
What retraction settings should I use for Prusament Prusament PETG 1.75mm on the Anycubic Kobra 2?
Use a retraction distance of 5.5 mm at 45 mm/s. These settings help reduce stringing and oozing during travel moves.
What fan speed should I use for PETG on the Anycubic Kobra 2?