PETG93% confidence

Best Settings for Prusament Prusament PETG 1.75mm on Prusa Mini+

Nozzle 240°C · Bed 85°C · 60 mm/s

Prusa Mini+ Specs

Max Nozzle Temp
280°C
Max Bed Temp
100°C
Hotend Type
PTFE-lined
Default Nozzle
0.4 mm
Build Volume
180×180×180 mm
Enclosure
Open frame
Release Year
2021

Prusament Prusament PETG 1.75mm Specs

Material
PETG
Nozzle Temp Range
230°C – 250°C
Bed Temp Range
70°C – 90°C
Diameter
1.75 mm
Spool Weight
1000 g
High-quality PETG with tight tolerances. Excellent layer adhesion, chemical resistance, and durability. Great for functional parts that need more strength than PLA.

Print Settings

0.4 mm nozzle· 0.2 mm layer height

93% confidenceSource: Manufacturer
Nozzle Temp
240°C
1st: 245°C
Bed Temp
85°C
1st: 85°C
Print Speed
60 mm/s
1st: 20 mm/s
Fan Speed
30%
ParameterValue
Nozzle Diameter0.4 mm
Layer Height0.2 mm
Nozzle Temperature240°C
Bed Temperature85°C
Print Speed60 mm/s
Retraction Distance3.5 mm
Retraction Speed35 mm/s
Fan Speed30%
EnclosureOptional

Notes

Mini+ + Prusament PETG: Bowden needs 3.5mm retraction for PETG. 240°C, 85°C bed. Built-in profile works. Use textured PEI.

Sources

Source type: Manufacturer

Where to Buy Prusament Prusament PETG 1.75mm

Prusament

Prusament PETG 1.75mm

Check price on PrusaBuy on Prusa

* Affiliate links — we may earn a commission at no extra cost to you. Learn more.

Related Settings

Frequently Asked Questions

What nozzle temperature should I use for Prusament Prusament PETG 1.75mm on the Prusa Mini+?
The recommended nozzle temperature is 240°C, with a first layer temperature of 245°C. This is based on a confidence score of 93%.
What bed temperature should I use for PETG on the Prusa Mini+?
Set your bed temperature to 85°C, with 85°C for the first layer.
What print speed should I use for Prusament Prusament PETG 1.75mm?
The recommended print speed is 60 mm/s, with a slower first layer speed of 20 mm/s.
Does printing PETG on the Prusa Mini+ require an enclosure?
No, an enclosure is not strictly required for printing PETG on the Prusa Mini+, though it can help in cold environments.
What retraction settings should I use for Prusament Prusament PETG 1.75mm on the Prusa Mini+?
Use a retraction distance of 3.5 mm at 35 mm/s. These settings help reduce stringing and oozing during travel moves.
What fan speed should I use for PETG on the Prusa Mini+?
Set your part cooling fan to 30%. Adjust lower for materials like ABS or ASA to reduce warping.