PETG85% confidence

Best Settings for Overture Overture PETG - Black on Bambu Lab A1

Nozzle 240°C · Bed 80°C · 120 mm/s

Bambu Lab A1 Specs

Max Nozzle Temp
300°C
Max Bed Temp
100°C
Hotend Type
all-metal
Default Nozzle
0.4 mm
Build Volume
256×256×256 mm
Enclosure
Recommended
Release Year
2023

Overture Overture PETG - Black Specs

Material
PETG
Nozzle Temp Range
230°C – 250°C
Bed Temp Range
70°C – 80°C
Diameter
1.75 mm
Spool Weight
1000 g
Color
Black
Overture PETG — tough and chemical-resistant with good layer adhesion. Dimensional accuracy ±0.05mm. Works well on textured PEI. 1.75mm, 1kg spool.

Print Settings

0.4 mm nozzle· 0.2 mm layer height

85% confidenceSource: Community
Nozzle Temp
240°C
Bed Temp
80°C
Print Speed
120 mm/s
Fan Speed
50%
ParameterValue
Nozzle Diameter0.4 mm
Layer Height0.2 mm
Nozzle Temperature240°C
Bed Temperature80°C
Print Speed120 mm/s
Retraction Distance1 mm
Retraction Speed40 mm/s
Fan Speed50%
EnclosureOptional

Notes

A1 + PETG: 100°C max bed is sufficient for PETG. Use smooth PEI or glue stick on textured.

Where to Buy Overture Overture PETG - Black

Overture

Overture PETG - Black

Check price on AmazonBuy on Amazon

* Affiliate links — we may earn a commission at no extra cost to you. Learn more.

Related Settings

Frequently Asked Questions

What nozzle temperature should I use for Overture Overture PETG - Black on the Bambu Lab A1?
The recommended nozzle temperature is 240°C. This is based on a confidence score of 85%.
What bed temperature should I use for PETG on the Bambu Lab A1?
Set your bed temperature to 80°C.
What print speed should I use for Overture Overture PETG - Black?
The recommended print speed is 120 mm/s.
Does printing PETG on the Bambu Lab A1 require an enclosure?
No, an enclosure is not strictly required for printing PETG on the Bambu Lab A1, though it can help in cold environments.
What retraction settings should I use for Overture Overture PETG - Black on the Bambu Lab A1?
Use a retraction distance of 1 mm at 40 mm/s. These settings help reduce stringing and oozing during travel moves.
What fan speed should I use for PETG on the Bambu Lab A1?
Set your part cooling fan to 50%. Adjust lower for materials like ABS or ASA to reduce warping.