TPU87% confidence

Best Settings for Overture Overture TPU - Black on Prusa MK4S

Nozzle 235°C · Bed 50°C · 25 mm/s

Prusa MK4S Specs

Max Nozzle Temp
290°C
Max Bed Temp
120°C
Hotend Type
all-metal
Default Nozzle
0.4 mm
Build Volume
250×210×220 mm
Enclosure
Recommended
Release Year
2024

Overture Overture TPU - Black Specs

Material
TPU
Nozzle Temp Range
210°C – 230°C
Bed Temp Range
30°C – 60°C
Diameter
1.75 mm
Spool Weight
1000 g
Color
Black
Overture TPU 95A — flexible filament for rubber-like parts. Shore 95A hardness. Best with direct-drive extruders at slow speeds (20–30mm/s). 1.75mm, 1kg spool.

Print Settings

0.4 mm nozzle· 0.2 mm layer height

87% confidenceSource: CommunityDry Filament First
Nozzle Temp
235°C
Bed Temp
50°C
Print Speed
25 mm/s
Fan Speed
100%
ParameterValue
Nozzle Diameter0.4 mm
Layer Height0.2 mm
Nozzle Temperature235°C
Bed Temperature50°C
Print Speed25 mm/s
Retraction Distance0.5 mm
Retraction Speed35 mm/s
Fan Speed100%
EnclosureOptional
Filament DryingYes — 50°C for 6h
Dry your filament before printing: 50°C for 6 hours. Moisture causes popping, stringing, and poor layer adhesion.

Notes

MK4S + TPU: Same as MK4. Excellent direct drive for flexibles. Print slowly.

Where to Buy Overture Overture TPU - Black

Overture

Overture TPU - Black

Check price on AmazonBuy on Amazon

* Affiliate links — we may earn a commission at no extra cost to you. Learn more.

Related Settings

Frequently Asked Questions

What nozzle temperature should I use for Overture Overture TPU - Black on the Prusa MK4S?
The recommended nozzle temperature is 235°C. This is based on a confidence score of 87%.
What bed temperature should I use for TPU on the Prusa MK4S?
Set your bed temperature to 50°C.
What print speed should I use for Overture Overture TPU - Black?
The recommended print speed is 25 mm/s.
Does printing TPU on the Prusa MK4S require an enclosure?
No, an enclosure is not strictly required for printing TPU on the Prusa MK4S, though it can help in cold environments.
Do I need to dry Overture Overture TPU - Black before printing?
Yes, dry this filament at 50°C for 6 hours before printing. Moisture causes stringing, popping, and poor layer adhesion.
What retraction settings should I use for Overture Overture TPU - Black on the Prusa MK4S?
Use a retraction distance of 0.5 mm at 35 mm/s. These settings help reduce stringing and oozing during travel moves.
What fan speed should I use for TPU on the Prusa MK4S?
Set your part cooling fan to 100%. Adjust lower for materials like ABS or ASA to reduce warping.