PLA95% confidence

Best Settings for Prusament Prusament PLA 1.75mm on Prusa Mini+

Nozzle 215°C · Bed 60°C · 80 mm/s

Prusa Mini+ Specs

Max Nozzle Temp
280°C
Max Bed Temp
100°C
Hotend Type
PTFE-lined
Default Nozzle
0.4 mm
Build Volume
180×180×180 mm
Enclosure
Open frame
Release Year
2021

Prusament Prusament PLA 1.75mm Specs

Material
PLA
Nozzle Temp Range
200°C – 220°C
Bed Temp Range
40°C – 60°C
Diameter
1.75 mm
Spool Weight
1000 g
Premium PLA with industry-leading ±0.02mm diameter tolerance. Consistent quality, excellent surface finish, and reliable prints every time. Made in-house by Prusa Research.

Print Settings

0.4 mm nozzle· 0.2 mm layer height

95% confidenceSource: Manufacturer
Nozzle Temp
215°C
1st: 220°C
Bed Temp
60°C
1st: 60°C
Print Speed
80 mm/s
1st: 25 mm/s
Fan Speed
100%
ParameterValue
Nozzle Diameter0.4 mm
Layer Height0.2 mm
Nozzle Temperature215°C
Bed Temperature60°C
Print Speed80 mm/s
Retraction Distance3.2 mm
Retraction Speed35 mm/s
Fan Speed100%
EnclosureOptional

Notes

Mini+ + Prusament PLA: Bowden setup needs higher retraction (3.2mm). Built-in PrusaSlicer profile is perfectly tuned. 215°C, 60°C bed.

Sources

Source type: Manufacturer

Where to Buy Prusament Prusament PLA 1.75mm

Prusament

Prusament PLA 1.75mm

Check price on PrusaBuy on Prusa

* Affiliate links — we may earn a commission at no extra cost to you. Learn more.

Related Settings

Frequently Asked Questions

What nozzle temperature should I use for Prusament Prusament PLA 1.75mm on the Prusa Mini+?
The recommended nozzle temperature is 215°C, with a first layer temperature of 220°C. This is based on a confidence score of 95%.
What bed temperature should I use for PLA on the Prusa Mini+?
Set your bed temperature to 60°C, with 60°C for the first layer.
What print speed should I use for Prusament Prusament PLA 1.75mm?
The recommended print speed is 80 mm/s, with a slower first layer speed of 25 mm/s.
Does printing PLA on the Prusa Mini+ require an enclosure?
No, an enclosure is not strictly required for printing PLA on the Prusa Mini+, though it can help in cold environments.
What retraction settings should I use for Prusament Prusament PLA 1.75mm on the Prusa Mini+?
Use a retraction distance of 3.2 mm at 35 mm/s. These settings help reduce stringing and oozing during travel moves.
What fan speed should I use for PLA on the Prusa Mini+?
Set your part cooling fan to 100%. Adjust lower for materials like ABS or ASA to reduce warping.